Match the following

Weld defect

Causes of defect

  P  

 Weld porosity

  1

 High welding current and low welding speed

  Q

 Slag inclusion

  2

 Insufficient heat and fast travel of troch

  R

 Weld crack

  3

 oxides, fluxes and electrode coating material

  S

 Weld spatter

  4

 Gases are trapped inside weld

  T

 Incomplete fusion

  5   

 Non uniform cooling and internal stresses

This question was previously asked in
ISRO Scientist ME 2011 Paper
View all ISRO Scientist ME Papers >
  1. P-4, Q-3, R-5, S-1, T-2 
  2. P-4, Q-2, R-3, S-5, T-1
  3. P-4, Q-5, R-1, S-2, T-3
  4. P-3, Q-5, R-2, S-1, T-4

Answer (Detailed Solution Below)

Option 1 : P-4, Q-3, R-5, S-1, T-2 
Free
ISRO Scientist Mechanical FT 1
95 Qs. 100 Marks 120 Mins

Detailed Solution

Download Solution PDF

Explanation:

Types of welding defects:

Weld porosity is due to atmospheric gases are trapped inside the liquid metal during the solidification of the metal.

Slag inclusion caused by trapping of the compound by oxides, fluxes and electrode coating materials in the weld zone.

Weld crack caused due to non-uniform cooling and internal stresses generated in weld Beed. If stress is more than the strength of the material cracks will be formed.

Weld spatter caused due to high welding current and low welding speed and arc blow.

Incomplete fusion caused due to insufficient heat and too fast/quick travel of torch or electrode.

Latest ISRO Scientist ME Updates

Last updated on Apr 14, 2023

The ISRO ( Indian Space Research Centre) released the official notification for the ISRO Scientist ME 2022 on 29th November 2022. The application window will remain open till 19th December 2022. A total of 33 vacancies have been released for the current recruitment cycle. The selected candidates for the post of ME in ISRO will get a basic salary of Rs. 56,100. Candidates who want a successful selection can refer to the ISRO Scientist ME Previous Year Papers to understand the level of the examination and improve their preparation accordingly. 

Hot Links: teen patti master 2023 teen patti royal teen patti all app teen patti plus real teen patti